Ferrite – Sintered

SINTERED FERRITE MAGNET DATA TABLES

Magnet Grade SFe Remanence Br kG (mT) Coercive Force Hc kOe (kA/m) Intrinsic Coercivity Hci kOe (kA/m) EnergyProduct BH max MGOe (kJ/m3) Density gram / cm3 Recoil Permeability
1336 2.5 2.1 3.6 1.3 4.8 1.2
  (250) (168) (288) (10.4)    
2033 3 2.5 3.3 2 4.8 1.1
  (300) (200) (264) (16.0)    
3031 3.5 3 3.1 3 4.8 1.1
  (350) (240) (248) (24.0)    
3635 3.9 3.2 3.5 3.6 4.9 1.1
  (390) (256) (280) (28.8)    
The temperature Coefficient of Br -0.20 % per degree C
The temperature coefficient of Hci 0.30 % per degree C
Maximum Operating Temperature 250 Degree C

The above mentioned magnet grades are but a few of the sintered ferrite grades available from Polaris REM. Sintered Ferrite magnets are anisotropic in nature. They are the lowest cost and most corrosion resistant magnet material. Sintered Ferrite magnetic properties are lower than those of isotropic bonded NdFeB magnets. Please contact PolarisREM with your specific requirements.